Skip to main content
. 2018 Dec 21;12(1):23. doi: 10.3390/ma12010023

Table 3.

Fracture energy obtained from DCB specimens oriented in RL by means of Compliance-Based Beam Method (CBBM).

Specimen Ref Ef (MPa) Pmax (N) C0 (mm/N) GI,Pmax (N/mm) GIc (N/mm)
140-1-RL 14,250 191.70 0.042 1.07 1.01
144-1-RL 15,203 173.00 0.040 0.81 0.84
144-2-RL 13,254 123.08 0.048 0.52 0.48
161-1-RL 12,266 172.35 0.047 0.97 0.95
161-3-RL 14,593 176.29 0.039 0.85 0.85
176-1-RL 14,557 151.70 0.042 0.65 0.61
176-2-RL 12,335 156.59 0.049 0.82 0.76
176-3-RL 11,577 183.95 0.048 1.10 1.02
189-1-RL 15,087 168.16 0.039 0.75 0.70
189-2-RL 12,293 177.06 0.045 0.95 0.92
192-1-RL 16,707 162.01 0.038 0.65 0.63
192-2-RL 14,399 147.76 0.044 0.70 0.65
192-3-RL 16,103 153.99 0.038 0.56 0.57
Mean 14,048 164.43 0.043 0.80 0.77
SD 1590 18.03 0.004 0.19 0.18
CoV (%) 11 11 10 23 23