Skip to main content
. 2018 Sep 28;3(11):2671–2678. doi: 10.1021/acsenergylett.8b01504

Table 1. PLQE of the Perovskite Thin Films Measured before and after Storage in Humid Nitrogen (50% RH) for 24 ha.

  PLQE (%)
sample before after
TC 18.6 27.9
Rb-passivated TC 22.8 12.9
K-passivated TC 39.5 49.6
a

Films were illuminated with a 532 nm laser at an excitation intensity equivalent to 1 sun (∼60 mW·cm–2).