Skip to main content
. 2019 Jan 28;9:810. doi: 10.1038/s41598-018-37123-3

Figure 11.

Figure 11

XRD spectra of degradation products on the surface of nHA_100, nHA_400, mHA_100, and mHA_400 coated Mg plates, as well as non-coated Mg plate control after immersion in rSBF for 6 weeks. XRD spetra of the representative nHA and mHA coatings before immersion were included for comparison. (a) nHA_100 and (b) nHA_400 after immersion, (c) nHA_400 before immersion, (d) mHA_100 and (e) mHA_400 after immersion, (f) mHA_400 before immersion, and (g) Mg plate after immersion. Mg plate samples had a dimension of 7.5 mm × 1 mm in diameter and thickness. Phases were identified based on MgO (ICSD pattern 01-077-2906), MgCO3∙3H2O (ICSD pattern 00-020-0669), CaCO3 (ICSD pattern 01-086-0174), HA (ICSD pattern 01-075-9526) and Mg (ICSD pattern 03-065-3365).