Skip to main content
. 2019 Jan 28;9:810. doi: 10.1038/s41598-018-37123-3

Figure 6.

Figure 6

Macroscopic images of nHA_100, nHA_400, mHA_100, mHA_400 coated Mg plates as well as non-coated Mg plate control at each prescribed time point during 6 weeks of immersion degradation in rSBF. Mg plates had a starting dimension of 7.5 mm in diameter and 1 mm in thickness. The plate samples before immersion is show in the 0 hr row.