Surface microstructures and elemental compositions of nHA_100, nHA_400, mHA_100, and mHA_400 coated Mg rods, as well as non-coated Mg rod control after immersion in rSBF for 6 weeks. SEM images of (a1) nHA_100, (a2) nHA_400, (b1) mHA_100, and (b2) mHA_400 coated Mg rods, and (c) non-coated Mg rod. The original magnifications for all images were 100x. (d) Surface elemental compositions (wt %) of each sample after immersion in rSBF for 6 weeks, quantified on the respective SEM images of a-c using EDS analyses. All Mg rod samples had an initial dimension of 7.5 mm in diameter and 15 mm in height.