Skip to main content
. 2019 Jan 24;15:218–235. doi: 10.3762/bjoc.15.21

Figure 8.

Figure 8

Integral distribution functions for the lamella thickness of crystallites in thermally fractionated (1) PCOE after Gr1 treatment, (2) PCOE/PNB blend, and NB–COE copolymers with different COE-block lengths, (3) LCOE = 22, (4) LCOE = 12, and (5) LCOE = 9.4 [92]