Cell viability and gain (average value±standard deviation) after labeling by silica‐coated Mn−Zn ferrite nanoparticles.

Labeling conc. [mM] BM‐MSCs[a] C6[a] AT‐MSCs[b]
Viability [%] Gain [%] Viability [%] Gain [%] Viability [%] Gain [%]
0.05 95±6 95±6 89±6 94±54 88±9 72±12
0.1 90±10 88±10 88±10 79±34 94±2 103±3
0.2 95±1 106±8
0.55 51±24[c] 66±8[c] 61±33 34±9
unlabeled cells 96±4 100±14 88±17 100±52 92±2 100±2

[a] 48‐hour labeling. [b] 24‐hour labeling. [c] Significantly differs from unlabeled cells (control).