. 2019 Jan 18;19(2):383. doi: 10.3390/s19020383

Figure 2.

Figure 2

Scanning electron microscopy (SEM) image of the cross-section of PZT-PWAS: (a) at room temperature; (b) after exposure to 250 °C temperature; (c) after exposure to 225 kGy nuclear radiation.