Skip to main content
. 2019 Jan 18;19(2):383. doi: 10.3390/s19020383

Figure 23.

Figure 23

Typical AE signals captured during fatigue crack growth. Three sets of captured signals are presented. For each set, the signal at PWAS 1 and the corresponding signal at PWAS 2 are presented. The AE signals seem to maintain their signature at PWAS 1 and 2.