Skip to main content
. 2019 Jan 18;9(1):116. doi: 10.3390/nano9010116

Figure 2.

Figure 2

SEM images of the solvent vapor annealing (SVA)-treated PCL/PEO fibers (a,a’) and PCL/PEO@PDA of different modification time intervals (b,b’), 5 h; (c), 30 h; (d,d’), 45 h; (e) UV-vis spectra of the PDA solution and PCL/PEO@PDA-45 fiber composite.