Skip to main content
. 2019 Jan 16;9(1):106. doi: 10.3390/nano9010106

Figure 7.

Figure 7

Cyclic voltammograms recorded at 5 mV·s−1 in 3 M H2SO4 and 0.15 M V(III)/V(IV) solution for CNFs derived from (A) KL; (B) KL loaded with Ketjen black.