Skip to main content
. Author manuscript; available in PMC: 2019 Aug 1.
Published in final edited form as: Addit Manuf. 2018 Jul 2;22:758–774. doi: 10.1016/j.addma.2018.06.024

Figure 2:

Figure 2:

Common defects and failures during metal-AM processing. (A) Pores in EBM Ti6Al4V prior to hot isostatic pressing [41] (B) Cracking and delamination in SLM M2-High Speed Steel [131](C) Microcrack formation and pores induced in SLM Hastelloy X, a Ni-based superalloy [132](D) Pores induced from keyhole laser effect in PBF SS316 stainless steel [44]. (E) Keyhole formation in laser processing of Ti6Al4V [45].