Fig. 2.

Fig. 2.

(A) In situ heating XRD patterns of Pt3Co/C annealed at various temperatures. The dashed line represents the as-synthesized Pt3Co/C alloy. (B) Calculated relative content of ordered intermetallic Pt3Co/C formed and particle size [calculated from the width of the (111) peak]. (C) In situ heating XRD patterns of Pt3Co/C at 750 °C, the optimal temperature, as a function of annealing time. (D) Calculated relative content of ordered Pt3Co/C formed and particle size.