Skip to main content
. 2019 Feb 8;10:399–411. doi: 10.3762/bjnano.10.39

Figure 10.

Figure 10

θ–2θ X-ray diffractogram for the Ti-thymine film deposited at 250 °C (black line), Ti-uracil deposited at 225 °C (blue line), and Ti-adenine 250 °C (red line). The reflections for the Ti-thymine film and their multiples are indicated by arrows.