Fig. 5.

Fig. 5

Carbon monoxide and carbon dioxide concentrations in the reactor. a After exposure of Zn-HPW/TiO2 to pure methane (CH4 0.3 MPa). The catalyst was regenerated by treatment in 1 bar of air under light at ambient temperature. b After exposure of Zn-HPW/TiO2 to CH4 and air. Reaction conditions: catalyst, 0.1 g; gas phase pressure, CH4 0.3 MPa, Air 0.1 MPa