The Brittleness and Stiffness of the Prepared Hot-Melt Extruded Filaments Were Determined by a Three-Point Bend Test Where the Distance (mm) Until the Filament Broke and Breaking Stress (g/mm2) Was Recorded and Used as an Indicator if the Filament Would Be 3D Printable (Mean ± SD, n = 10)

Formulation Breaking distance (mm) Breaking stress (g/mm2) Printable
PLA 3.69 ± 0.28 15,361.45 ± 2064.55 Yes
1 2.39 ± 0.43 5456.12 ± 769.68 Yes
2 1.93 ± 0.13 3125.75 ± 185.30 Yes
3 3.50 ± 1.09 5046.78 ± 1324.55 Yes
4 0.83 ± 0.05 3145.73 ± 265.98 No
5 2.80 ± 0.62 4982.93 ± 604.85 Yes
6 0.90 ± 0.19 1334.48 ± 67.08 No
7 2.70 ± 0.47 5119.04 ± 369.75 No
8 4.07 ± 0.94 4662.66 ± 625.93 No*
9 1.24 ± 0.13 4251.27 ± 929.07 No
10 2.59 ± 0.32 3255.59 ± 294.42 Yes
11 2.31 ± 0.31 4988.52 ± 142.70 Yes
12 1.78 ± 0.26 7637.32 ± 808.91 Yes
13 2.93 ± 0.28 6496.31 ± 443.79 Yes

*Day-to-day variability regarding printability, as the filament deformed during feeding, which occasionally failed the prints