Spatially resolved polarization switching of variable-thickness BiFeO3 following TAFM. (A) BiFeO3 film thickness (h) and (B) cross-sectional HAADF-STEM of BiFeO3 following TAFM showing unperturbed crystal structure. (C) Coercive voltage, Vc and (D) coercive field, Ec cospatial with A, determined at the onset of ferroelectric switching from P to P+ polarization.