Skip to main content
. 2019 Feb 19;10:841. doi: 10.1038/s41467-019-08835-5

Table 1.

Comparison of TE performance of flexible n-type TE materials at room temperature

Materials α (μV K−1) σ (S cm−1) PF (μW m−1 K−2) Ref.
Ag2Te/copy-paper −100 85 85 21
Cu-doped Bi2Se3/PVDF −84 146 103.2 43
Ni NWs/PVDF −20.6 4700 200 44
Bi2Te3/Cellulose fiber −130 148 250 23
C60/TiS2 −101 390 400 40
HgSe −518 20 550 22
TiS2[tetrabutylammonium]0.013[hexylammonium]0.019 −150 400 904 45
Ag2Se/Nylon membrane −140 497 987 This work