Skip to main content
. 2019 Feb 3;12(3):471. doi: 10.3390/ma12030471

Figure 6.

Figure 6

SEM micrographs of (a) PP/TPS/MA blend [184]; (b) TPS/PE compatibilized with PP-g-MA 20%—scale 20 μm [186]; (c) 30TPS/70PA12 blend [190]; (d) LDPE/PHB 80:20—scale 40 μm [191]; (e) PS45/PHB45-(block copolymer) C10 blend [192]; (f) PLA/PS (0.3 volume fraction) blend [193].