Table 5.
Optimized Parameter | ME Galfenol-PZT | ME Metglas-PZT | MME PZT Bimorh | |||
---|---|---|---|---|---|---|
ICNIRP | IEEE | ICNIRP | IEEE | ICNIRP | IEEE | |
21.5 mm | 2 mm | 25.2 mm | 2 mm | NA | NA | |
15.9 µm | 19.4 µm | 18.1 µm | 25.5 µm | 10 µm | 10 µm | |
33.5 µm | 40.3 µm | 22.4 µm | 37.3 µm | NA | NA | |
1.1 mm | 10 mm | 1.26 mm | 10 mm | 0.4 mm | 0.51 mm | |
0.44 Oe | 2.89 Oe | 0.40 Oe | 2.89 Oe | 5.56 Oe | 38.39 Oe | |
NA | NA | NA | NA | 8.0 mm | 8.0 mm | |
NA | NA | NA | NA | 0.48 mm | 0.39 mm | |
NA | NA | NA | NA | 5.0 mm | 5.0 mm | |
65 kHz | 698 kHz | 71.9 kHz | 915 kHz | 61 Hz | 325 Hz | |
15.6 µW | 7.4 mW | 62.6 µW | 42.7 mW | 120 µW | 8.7 mW |