. 2019 Feb 8;12(3):516. doi: 10.3390/ma12030516

Figure 7.

Figure 7

Figure 7

Distribution of martensite (a,c) and bainite (b,d) phases after hybrid welding of S700MC steel T-joints with a thickness of 10 mm (cross-sections were made in the half-length of the joint).