Comparison of Martens hardness (HM) values for samples before and after thermal treatment at 170°C for 1 h.

Sample HM
25°C 170°C (1h)
PP 31 490
PP/GRA1 548 653
PP/GRA2 378 405
PP/GRA1Ti 191 146
PP/GRA2Zn 269 224