Table 3. TP values and paired t-test results of materials between before and after glazing in 0.6 mm and 1.0 mm thickness.
Material | Not glazed | Glazed | P value | Increased percentage | ||
---|---|---|---|---|---|---|
Mean | SD | Mean | SD | |||
0.6 mm EM | 30.37 | 1.31 | 35.07 | 1.53 | .000* | 15.48 |
0.6 mm ZP | 33.03 | 1.79 | 34.10 | 1.43 | .157 | 3.24 |
1.0 mm EM | 19.77 | 2.05 | 21.76 | 2.75 | .084 | 10.07 |
1.0 mm ZP | 24.52 | 0.86 | 24.72 | 1.12 | .652 | 0.82 |
EM: IPS e.max Press, ZP: IPS e.max ZirPress.
*Significantly different compared to test groups (P < .05)