Skip to main content
. 2018 Dec 21;11(1):11. doi: 10.3390/polym11010011

Figure 7.

Figure 7

Relative resistance change (R/R0) during single loading-unloading cycle for (a) linear axial and (b) linear transverse sensors tested under various maximum strains ranging from 10% to 100%. The R/R0 response of 100% maximum strain loading in (a) is plotted against the secondary ordinate.