Figure 2.

Figure 2

Apparent viscosity as a function of shear rate for (a) PGSA-co-PEGDA in various degree of acrylation; (b) PGSA-co-PCLDA in various degree of acrylation; (c) PEGDA, PCLDA, and PGSA prepolymers in various degree of acrylation. Note that PCLDA was measured at 40 °C instead of 25 °C according to the printing parameter of Cheng et al. [34].