Skip to main content
. 2019 Jan 9;11(1):102. doi: 10.3390/polym11010102

Table 1.

Crystallinity of PP and PP/TH composites before and after UV accelerated weathering.

Sample Before After
Hm Xc Tm Hm Xc Tm
(J/g) % °C (J/g) % °C
PP −71.6 34.6 165.0 −53.3 25.7 163.3
5TH −74.9 38.1 166.5 −72.0 36.6 166.8
10TH −75.6 40.6 164.1 −62.0 33.3 167.6
15TH −71.3 40.5 164.0 −57.7 32.8 164.7
30TH −59.1 40.8 164.2 −49.6 34.2 165.1