. 2018 Dec 6;10(12):1353. doi: 10.3390/polym10121353

Figure 5.

Figure 5

Selected 2D WAXS patterns of PLLA/PDLA-60-2 fibers during heating to 210 °C (a) and 215 °C (b), and the following cooling process.