Skip to main content
. 2018 Dec 1;10(12):1329. doi: 10.3390/polym10121329

Figure 9.

Figure 9

(a) DPV peak current response of RGO/Fe3O4-IL-MIP sensor after incubating in 20 μM DPA and its analogs (n = 3). (b) DPV peak current response of RGO/Fe3O4-IL-MIP sensor after incubating in 20 μM DPA and 20 μM DPA in the presence of other analogs (n = 3). (c) The chemical structures of DPA (a’) and its analogs of 2-nitroaniline (b’), 3-nitroaniline (c’), 4-nitroaniline (d), benzene (e), 1,2-dimethylbenzene (f), 1,4-phenylenediamine (g), hydroquinone (h), catechol (i), 1-naphthylamine (j), and phenol (k).