Skip to main content
. 2018 Dec 11;10(12):1371. doi: 10.3390/polym10121371

Figure 6.

Figure 6

Stacked DSC (endo up) of the melting peak of PHBV:PLA blends with increasing wt.% of CB: (a) PHBV:PLA = 100:0, (b) PHBV:PLA = 90:10, (c) PHBV:PLA = 80:20, and (d) PHBV:PLA = 60:40.