The impact properties of neat PLA, PLA/PBS and PLA/PBS/EGMA blends: (A) impact strength; (BC) deformed impact samples: (a) neat PLA; (b) PLA/PBS 70/30; (cf) PLA/PBS/EGMA (70/30/x): (c) 5 wt %; (d) 10 wt %; (e) 15 wt %; (f) 20 wt %.