Skip to main content
. 2019 Jan 15;11(1):141. doi: 10.3390/polym11010141

Figure 3.

Figure 3

SEM images of electrospun fibers obtained from GG solutions with concentration of: (A) 1.1 wt %; (B) 1.3 wt %; (C) 1.5 wt %; (D) 1.7 wt %; (E) 1.9 wt %; (F) 2.0 wt %; (G) 2.1 wt %; and (H) 2.2 wt %. Magnification is 10,000×.