Skip to main content
. 2019 Jan 15;11(1):141. doi: 10.3390/polym11010141

Figure 4.

Figure 4

SEM images and fiber diameter size (FDS) of electrospun fibers obtained from GG solutions at 2 wt % concentration loaded with: 5 wt % TA (A); 10 wt % TA (B); 15 wt % TA (C); and 20 wt % TA (D). Magnification is 10,000×.