Thermodynamic properties of the neat GG and GG fibrous mats loaded with TA.

Sample GG-powder GG-fiber 10% TA 15% TA 20% TA
Tm (°C) 318 298 301 300 293
ΔH (J/g) 47.76 82.14 49.68 37.53 122.10