Skip to main content
. 2018 Oct 11;10(10):1129. doi: 10.3390/polym10101129

Figure 15.

Figure 15

UV-VIS spectra of PDMS–TiO2 hybrid films for different TIP/PDMS–OH molar ratios (shown in the legend), using PDMS–OH precursors with viscosities of (a) 25; (b) 65; and (c) 750 cSt, corresponding to average molar masses of 2100, 4000, and 20,000 g mol−1, respectively (calculated based on experimental measurements from [85]). Reproduced with permission from Dalod et al. Nanomaterials; published by MDPI, 2017.