Figure 6.

Figure 6

SEM images of char residue after cone calorimeter test: (A1,A2) the outer surface and the inner surface of PLA/IFR; and (B1,B2) the outer and inner surface of PLA/IFR/α-ZrP2 (Adapted with permission from [81].