Skip to main content
. 2018 Oct 2;10(10):1092. doi: 10.3390/polym10101092

Figure 5.

Figure 5

Comparison of surface weight percentage measured by XPS (white bar), with overall LC measured by UV-Vis (black bar) for samples, PCL-CAF1.5-W and PCL-CAF1.5-Ac, produced at FR = 20 mL/min.