Table 1.
Yield (%) | Inherent Viscosity a (dL/g) | DI b (%) | Thermal Properties (°C) | ||
---|---|---|---|---|---|
T5 c | T10 d | Tg e | |||
97 | 0.15 | 95 | 476 | 513 | 352 |
a Measured at a concentration of 0.5 g/dL in concentrated sulfuric acid at 30 °C. b Degree of imidization calculated from FT-IR spectra using Equation (1). c Temperature at which a specimen shows 5 wt % decomposition under N2. d Temperature at which a specimen shows 10 wt % decomposition under N2. e Glass transition temperature measured under N2.