Figure 7.

Figure 7

DMTA of PK-Fu crosslinked with b-Ma (PK-Fu/B-Ma, filled red squares) and PK-Fu crosslinked with B-Ma and reinforced with 5 wt.% of MWCNTs before (PK-Fu/B-Ma/MWCNT, filled black squares) and after resistive heating annealing (PK-Fu/B-Ma/MWCNT, black empty squares) for 24 h using 35 V.