Figure 10.

Figure 10

Stress–strain curves of different solution concentrations. The collecting time of the fiber mats was set to 120 min. The processing parameters were as follows: Applied voltage of 20 kV, working distance of 20 cm, and flow rate of 1.0 mL/h.