Table 2.
Melting and crystallization temperatures determined from DSC.
Sample | Silk Composition | T c1 | T c2 | T m1 | T m2 | Td (°C) |
---|---|---|---|---|---|---|
HNS0 | 0% | 189.5 | 197.3 | 189.0 | 197.5 | - |
HNS10 | 10% | 191.4 | 198.4 | 190.6 | 198.8 | 290 |
HNS25 | 25% | 192.4 | 199.4 | 192.0 | 200.3 | 287 |
HNS50 | 50% | 194.5 | 200.8 | 193.5 | 201.5 | 272 |
HNS75 | 75% | 192.1 | 200.7 | 191.1 | 201.2 | 270 |
HNS90 | 90% | 190.3 | 200.5 | 189.1 | 200.1 | 269 |
HNS100 | 100% | - | - | - | - | 267 |