Skip to main content
. 2018 Oct 12;10(10):1134. doi: 10.3390/polym10101134

Table 3.

Spinning parameters of the produced PVDF hollow fibers (HFs).

Spinning Condition
Dope temperature 80 °C
Dope flow rate 11–12 g/min
Bore fluid composition and flow rate NMP 30%; 13 g/min
Bore fluid temperature 50 °C
Outer coagulant Tap water at room temperature
Air gap 24 cm
Spinneret dimension O.D.–I.D. 1.6–0.6 mm

O.D.: outer diameter; I.D.: inner diameter.