Skip to main content
. 2018 Oct 4;10(10):1098. doi: 10.3390/polym10101098

Figure 1.

Figure 1

(A) The size distributions of the N-isopropylacrylamide/sodium copper chlorophyllin (NIPAAm/SCC) nanogels with various SCC concentrations; (B) the size distributions of NIPAAm/NHMAAm/SCC nanogels containing 1% SCC with different NIPAAm/N-(hydroxymethyl)acrylamide (NHMAAm) ratios; (C) a transmission electron microscope (TEM) image of p(NIPAAm-co-NHMAAm-co-SCC) nanogels (80/19/1) counterstained with phosphotungstic acid (average size: 133 ± 30 nm, n = 120).