Skip to main content
. 2018 May 28;10(6):592. doi: 10.3390/polym10060592

Figure 6.

Figure 6

The variation of the Water Contact Angle test of cellulose and cellulose-g-PNIPAAm with different graft degrees at 25 °C and 45 °C, respectively (a); Reversible WCA transition of the product at 25 °C and 45 °C, respectively (b).