Skip to main content
. 2018 May 23;10(6):573. doi: 10.3390/polym10060573

Figure 11.

Figure 11

(A) An illustration of the synthesis process of a stretchable conductor on an elastomer substrate; (B) the optical microscopy images of copper layers of ELD on rubber at different tensile strains (from 0% to 70%) [37].