Skip to main content
. 2018 Jun 11;10(6):651. doi: 10.3390/polym10060651

Figure 8.

Figure 8

Mechanical properties and water resistance of the particleboards bonded by the tannin–sucrose–sulfuric acid adhesive (pH 1.0) and the tannin–sucrose adhesive (pH 4.8) at 180 °C for 10 min. (a) Bending properties; (b) internal bond (IB) strength properties; and (c) thickness swelling (TS) properties. MOR—modulus of rupture.