Table 11.
Selected CM results with cavity-size engineered ArMs.
![]() | ||||
| entrya | catalyst | substrate | conversionb (%) | TON |
| 1 | ArM 5 | 73 | >99c | 100 |
| 2 | ArM 6 | 73 | >99c | 100 |
| 3 | ArM 7 | 73 | 69c | 69 |
| 4 | 9 | 73 | 79c | 79 |
| 5 | 9 + NB4exp | 73, 74, 75 | 0 | 0 |
| 6 | ArM 5 | 74 | 45c | 45 |
| 7 | ArM 6 | 74 | >99c | 100 |
| 8 | ArM 7 | 74 | >99c | 100 |
| 9 | 9 | 74 | 98d | 98 |
| 10 | ArM 5 | 75 | 40d | 40 |
| 11 | ArM 6 | 75 | >99d | 100 |
| 12 | ArM 7 | 75 | >99d | 100 |
| 13 | 9 | 75 | 94d | 94 |
a[Substrate] = 0.05 M. bConversions determined by 1H NMR. cE/Z = 20:1. dE/Z = 99:1.