Table 5.

Permeability values in terms of water vapor permeability (WVP) and d-limonene permeability (LP) for the electrospun films of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) and PHBV/Mobil Composition of Matter (MCM)-41 with eugenol.

Sample WVP × 10−14 (kg·m·m−2·Pa−1·s−1) LP × 10−14 (kg·m·m−2·Pa−1·s−1)
PHBV 5.34 ± 1.79 2.68 ± 1.82
PHBV/2.5 wt.-% MCM-41 + eugenol 8.68 ± 3.57 3.41 ± 0.97
PHBV/5 wt.-% MCM-41 + eugenol 8.84 ± 4.36 3.49 ± 1.17
PHBV/7.5 wt.-% MCM-41 + eugenol 4.25 ± 4.04 3.51 ± 0.54
PHBV/10 wt.-% MCM-41 + eugenol 2.99 ± 0.95 2.32 ± 0.68
PHBV/15 wt.-% MCM-41 + eugenol 0.25 ± 0.19 0.38 ± 0.20
PHBV/20 wt.-% MCM-41 + eugenol 4.08 ± 1.98 4.66 ± 2.91