Chemical compositions (wt.%) of oxides and elements obtained by XRF analysis of the original gold ore (before incubation) and the solid residue (after incubation).

Sample type Bacterial strain Chemical compositions of oxides and elements, wt.%
SiO2 SO3 Pb Al2O3 Fe2O3 CaO K2O ZnO Au MgO Ag Cr2O3 LOI
Original ore sample before the microbial treatment 78.6 4.57 3.37 3.47 3.12 2.92 1.64 0.82 0.26 0.24 0.20 0.16 0.61
Ore samples (solid residue) after the microbial treatment with each bacterial strain a-1 85.6 4.07 2.3 2.15 1.97 1.49 1.07 0.49 0.00 0.16 0.14 0.24 0.32
a-2 82.6 2.82 3.43 2.63 2.58 2.75 1.38 0.80 0.12 0.25 0.14 0.20 0.32
e-1 83.1 4.63 3.00 2.18 2.35 2.09 1.17 0.66 0.10 0.15 0.13 0.15 0.29
e-2 82.8 5.07 2.58 2.35 2.36 2.28 1.30 0.63 0.00 0.16 0.13 0.11 0.23
f-1 83.8 5.03 3.00 2.09 1.82 1.48 1.23 0.56 0.00 0.13 0.17 0.33 0.36
f-2 79.1 6.23 3.30 2.50 2.90 2.31 1.56 0.90 0.18 0.23 0.00 0.27 0.40
j-1 85.3 5.05 2.4 1.97 1.46 1.62 1.09 0.38 0.03 0.13 0.09 0.24 0.24
j-2 83.7 4.40 2.73 2.07 2.54 1.70 1.09 0.62 0.04 0.16 0.13 0.21 0.61
NC* 83.1 4.82 2.78 2.29 1.98 2.27 1.13 0.49 0.26 0.15 0.12 0.21 0.38

The Au content of the original ore sample used in this study was 0.26 wt.%. *NC: Negative Control.