. 2018 Feb 13;10(2):183. doi: 10.3390/polym10020183

Figure 7.

Figure 7

TEM images of (a) thin-walled GCEINs and (b) thick-walled GCEINs in sample KL/Fe-800. The structural defects in the graphitic-carbon shells are indicated by arrows.