Skip to main content
. 2018 Feb 11;10(2):176. doi: 10.3390/polym10020176

Figure 3.

Figure 3

Figure 3

Effect of: urea concentration (A); and SDS amount (B) on the adhesive strength of modified spent hen protein. Curing conditions: time = 4 min; temperature = 110 °C; pressure = 3.5 MPa. Figure adopted with copyright permission from Elsevier (for Wang and Wu, 2012).